Publication

Semiconductor & Quantum Packaging Laboratory

Journal

2006 Evaluation of solder joint reliability in flip chip package under thermal shock test

페이지 정보

작성자 최고관리자 작성일 25-09-15 15:50

본문

Author
Dae-Gon Kim, Jong-Woong Kim and Seung-Boo Jung
Journal
Thin Solid Films
Vol
504
Page
426
Year
2006
IF
1.761

The microstructural investigation and thermo-mechanical reliability evaluation of the Sn–3.0Ag–0.5Cu solder bumped flip chip package were carried out during the thermal shock test of the package. In the initial reaction, the reaction products between the solder and electroless Ni–P bump of the chip side were composed of two layers, i.e., a continuous layer of (Ni,Cu)3Sn4 and discontinuous particles of (Cu,Ni)6Sn5, while a continuous (Ni,Cu)3Sn4 IMC layer was formed between the solder and electroless Ni–P layer of the package side. It is found that the primary failure mechanism of the solder joints in this type of test was thermally activated solder fatigue failure. For the interpretation of the failure mechanism of the package, finite element analyses were also conducted. The finite element analyses revealed that the cracks were induced by the accumulation of the plastic work and creep strain. Inelastic strain accumulations are primarily affecting the crack initiation and growth time, so called the life of the solder joint in this thermal shock test condition.