2005 olid state interfacial reaction and joint strength of Sn-37Pb solder with Ni-P under bump metallization in flip chip application

페이지 정보

작성자 최고관리자 작성일 25-09-15 15:29

본문

Author
Dae-Gon Kim, Jong-Woong Kim, Jung-Gu Lee, Hirotaro Mori, David J. Quesnel and Seung-Boo Jung
Journal
Journal of Alloys and Compounds
Vol
395
Page
80
Year
2005
IF
3.014

The interfacial microstructure of Sn–37Pb solder with immersion Au/electroless Ni–P under bump metallization (UBM) was studied using scanning electron microscopy (SEM) and transmission electron microscopy (TEM). A Ni3Sn4 intermetallic compound (IMC) layer was formed at the interface between the solder and Ni–P UBM upon reflow. However, after isothermal aging, AuSn4 containing a certain amount of Ni dissolved in it, i.e. (Au,Ni)Sn4, appeared above the Ni3Sn4 layer. Two distinctive layers, P-rich and Ni–Sn–P, were additionally found from the TEM observation. Analytical studies using energy dispersive spectrometer (EDS) equipped in TEM revealed that the averaged composition of the P-rich layer is more close to that of a mixture of Ni3P and Ni, while that of the Ni–Sn–P layer is analogous to the P-rich layer but containing a small amount of Sn in it. The growth of the Ni3Sn4 IMC layer thickness obeyed a parabolic growth law which implies that the interfacial IMC growth is mainly controlled by volume diffusion of the elements to the reaction layer. The shear force of the joints decreased during isothermal aging at 373 K. The decrease of the shear force could be mainly due to the coarsening effect of the microstructure within the solder. The failure behavior could be well explained with the results of finite element modeling (FEM) analyses.