2006 Characteristic analysis of electroless Ni plating layer for electronic packaging

페이지 정보

작성자 최고관리자 작성일 25-09-15 15:51

본문

Author
Dae-Gon Kim, Jong-Woong Kim, Jeong-Won Yoon, Won-Bae Lee, Seung-Boo Jung
Journal
Surface and Interface Analysis
Vol
38
Page
440
Year
2006
IF
1.018

The crystallization behavior of electroless Ni–P film was investigated using X-ray diffractometry (XRD), transmission electron microscopy (TEM) and differential scanning calorimetry (DSC). XRD analyses revealed that the amorphous state of the as-plated Ni–P film was crystallized by heat treatment at 573 K for 1 h. Two peaks were observed simultaneously, indicating Ni and Ni3P compounds. Convergent beam electron diffraction (CBED) pattern analyses confirmed a size of the Ni3P in the crystallized Ni–P layer of 50–70 nm. The contact resistance decreased with a heat treatment, which is mainly due to the crystallized Ni–P layer and the grain growth. The activation energy calculated from DSC analyses using the Kissinger equation was 195.2 kJ/mol. Copyright © 2006 John Wiley & Sons, Ltd.